直连绳索取心钻杆分区热处理技术研究
作者:
作者单位:

1.金石钻探(唐山)股份有限公司,河北 唐山 063000;2.吉林大学建设工程学院,吉林 长春 130026;3.自然资源部复杂条件钻采技术重点实验室,吉林 长春 130026

作者简介:

通讯作者:

中图分类号:

P634

基金项目:

自然资源部复杂条件钻采技术重点实验室与金石钻探(唐山)股份有限公司2023 开放课题;国家自然科学基金项目(编号:42172345);吉林大学研究生创新基金资助项目(编号:2024CX103)


Research on zone heat treatment technology of straight-connected wire-line core drill pipe
Author:
Affiliation:

1.Jinshi Drill Tech Co., Ltd., Tangshan Hebei 063000, China;2.College of Construction Engineering, Jilin University, Changchun Jilin 130026, China;3.Key Laboratory of Drilling and Exploitation Technology in Complex Conditions, Ministry of Natural Resources (Jilin University), Changchun Jilin 130026, China)

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    为了提高绳索取心钻杆的性能,对直连绳索取心钻杆的受力情况、结构特点以及传统处理工艺进行分析,提出了分区热处理的工艺。通过对两端进行热加工处理,使钻杆中间管体区域和两端热处理螺纹区域性能出现差异,提高两端综合强度的同时改善螺纹部分的受力状态,可使钻杆柱既具有高强度又兼具柔性,大幅提高钻杆机械性能以及耐磨性。其中调质硬度HRC33~38能在保证管体延伸率与正火、回火基本一致的情况下,强度提高37.7%,硬度提高40%,抗冲击性提高46.7%。调质硬度HRC38~42时,材料的耐磨性提高9.1%。更适合全液压钻机施工及深孔钻进,为钻探施工提供了钻机、钻杆配套性的优选方案。

    Abstract:

    In order to improve the performance of the wire-line core drill pipe, the stress, structural characteristics and traditional treatment technology of the straight-connected wire-line core drill pipe were analyzed, and a zonal heat treatment process was proposed. Through the heat treatment of both ends, the heat treatment performance of the middle pipe body area and the thread area at both ends was different, and the comprehensive strength of both ends was improved while the stress state of the thread part was improved. It can make the drill pipe string have both high strength and flexibility, and greatly improve the mechanical properties and wear resistance of the drill pipe. The quenching and tempering hardness HRC33~38 can increase the strength by 37.7%, the hardness by 40% and the impact resistance by 46.7% under the condition that the elongation of the pipe body is basically the same as that of normalizing and tempering. When the quenching and tempering hardness is HRC38~42, the wear resistance of the material is increased by 9.1%. It is more suitable for full hydraulic drilling rig construction and deep hole drilling, and provides the optimal scheme for drilling rig and drill pipe matching.

    参考文献
    相似文献
    引证文献
引用本文

何蕙岚,王久全,李秋玥,等.直连绳索取心钻杆分区热处理技术研究[J].钻探工程,2024,51(3):125-130.
HE Huilan, WANG Jiuquan, LI Qiuyue, et al. Research on zone heat treatment technology of straight-connected wire-line core drill pipe[J]. Drilling Engineering, 2024,51(3):125-130.

复制
分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2023-12-17
  • 最后修改日期:2024-04-01
  • 录用日期:2024-04-02
  • 在线发布日期: 2024-05-30
  • 出版日期: 2024-05-10